Kuberako ibyiza byagusudira, nkibisobanuro bihanitse, gukora neza, imikorere yoroshye kandi yoroshye, bikoreshwa mubikorwa byinshi kandi byinshi, ariko hazabaho kandi inenge zimwe murwego rwo gusudira, biganisha ku gusudira kudatunganye, uburyo bwo kugabanya cyangwa kwirinda kuvuka kwibi bibazo, kubona igisubizo cyavunaguye nabakora umwuga wo gusudira wabigize umwuga.
Ibisubizo by'ibice:
Ibibyimba bikozwe mu gusudira imashini yo gusudira ya lazeri ahanini ni ibice bishyushye, nk'ibisasu bya kristu, ibice byo gutembera, n'ibindi, impamvu yabyo ni uko gusudira bitanga imbaraga nini zo kugabanuka mbere yo gukomera byuzuye, kuko iki cyuho gishobora kuba kugabanya cyangwa gukurwaho wuzuza insinga, gushyushya izindi ngamba.
Ibisubizo ku myobo yo mu kirere:
Gusudira kwinshi bikunda guhura nikibazo cyo kwikinisha, ibi biterwa nuko pisine yo gusudira ya laser ari ndende kandi ifunganye, igipimo cyo gukonjesha kirihuta cyane, kandi gaze ikomoka muri pisine yashongeshejwe ntigifite umwanya uhagije wo guhunga, bikavamo gushiraho ya porosity.Nyamara, gusudira lazeri birakonja vuba, kandi ububobere bwakozwe muri rusange ni buto ugereranije nubwa gakondo bwo gusudira.Ubuso bwakazi bushobora gusukurwa mbere yo gusudira kugirango ugabanye imyenge, kandi icyerekezo cyo guhuha nacyo kizagira ingaruka kumyuka.
Umuti wo gutatanya:
Kumeneka bikozwe na laser yo gusudira ntabwo bizanduza gusa kandi byangiza lens, ariko kandi bizagira ingaruka zikomeye kubuso bwa weld.Igisekuru cya spatter gifitanye isano cyane nubucucike bwingufu, kandi kugabanuka gukwiye kwingufu zo gusudira birashobora kugabanya spatter.Niba kwinjira bidahagije, umuvuduko wo gusudira urashobora kugabanuka.
Ibisubizo byo kuruma ku nkombe:
Niba umuvuduko wo gusudira wihuta cyane mu gusudira, icyuma gisukuye inyuma yumwobo muto werekeza hagati ya weld ntigifite umwanya wo kugabana, kandi gukomera kumpande zombi za weld bizakora impande zombi.Icyuho cyo guteranya hamwe ni kinini cyane, gushonga ibyuma bya kawusi biragabanuka, kandi impande ziroroshye kurumwa.Kurangiza gusudira laser, niba ingufu zo kugabanuka zihuta cyane, umwobo muto uroroshye gusenyuka, bikaviramo kuruma kwaho, kugenzura imbaraga no guhuza umuvuduko birashobora kuba igisubizo cyiza kubyara.
Igisubizo cyibisenyuka bitanu:
Niba umuvuduko wo gusudira utinda, pisine yashongeshejwe ni nini kandi yagutse, ubwinshi bwibyuma bishongeshejwe byiyongera, kandi uburemere bwubuso buragoye kubungabunga ibyuma biremereye byamazi, ikigo cyo gusudira kizarohama, gisenyuka no mu byobo.Muri iki gihe, birakenewe kugabanya neza ubwinshi bwingufu kugirango wirinde kugwa kwa pisine yashongeshejwe.
Impamvu zibibazo bitandukanye byo gusudira laser ziratandukanye, kandi tugomba mbere na mbere gushaka impamvu zo gusesengura ibibazo kugirango tubone uburyo bukwiye.Ibindi bijyanye nibisanzwe byo gusudira byimashini yo gusudira laser ikaze gusura urubuga rwacu kugirango ubyumve.Isosiyete yacu itanga ubwoko bwose bwimashini yo gusudira laser,imashini ikata laser, ibikoresho bya mashini ya laser, ibyitegererezo byuzuye, ubuziranenge bwizewe, serivisi nziza, guhangayika kubusa nyuma yo kugurisha.